Dear Mohammed,

Thank you for your response.

We're facing another significant issue.

Most of our carbon steel Procedure Qualification Records covering groups G1-G2, G1-G3 & G2-G3, G3-G3 with various process combinations are showing an unacceptable hardness range (260–325 HV) in the Heat-Affected Zone.

Our maximum acceptable hardness limit is 250 HV.

We've used different testing agencies, yet the results remain consistently high.


Regards,

Saurabh


On Fri, 17 Oct 2025 at 8:26 AM, Mohmmed Dudhiyawala <mdudhiya007@gmail.com> wrote:
Dear Saurabh,
Refer Table A.12 of NACE MR0175/ISO 15156, where Inconel 625 is designated as Type 4d.
Refer Table A.14. From Temp<149°C, Inconel 625 can be used for all conditions, stipulated in table. Hardness to be limited to 40 HRC max. (392 HV).


Regards,
Mohammed

On Tuesday, August 19, 2025 at 7:47:46 AM UTC+5:30 Saurabh Jain wrote:
Dear experts.

I am currently in the process of qualifying a PQR for API 5L X65 + A350 LF6. Both material consists of a base metal with alloy 0625 cladding. Welding process: GTAW+SMAW

During the mechanical testing, I witnessed the following hardness values:
Clad material: 300 to 390 HV
Weld metal: 280 to 350 HV

This is for Aramco project, so I referred their standard 01-SAMSS-044, and it specifies that I must refer to NACE MR0175/ISO 15156 for hardness acceptance criteria, particularly for the clad.

I have reviewed the standard but cannot find a specific acceptable hardness range. I also checked Aramco's W-11/W-12 and W-16 standards but was unable to find the maximum allowable hardness for clad welding.

My question is: Are these recorded hardness values for the clad and weld metal acceptable under the NACE MR0175/ISO 15156 standard? If not, what are the typical hardness limitations and under which standard?

Regards 
Saurabh Jain

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/a43d8910-6d95-4287-be8b-e6b26c0728d5n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CADr-LL9ApTuUqw3Y-s-PVrqAMSwrEsjoxKx3Joh%2BGV-MZ3hPmQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .