Re: [MW:35037] waiting period between welding and NDT

In my understanding, the code  is silent. Check client spec


On Mon, May 13, 2024 at 6:44 PM Ali Aghajafari <aghajafari.ins@gmail.com> wrote:
Hi all,

Is there a waiting period between welding and NDT in the ASME Code in order to find cold cracking. Material is SA 182 Gr. F12

Thanks for your answers

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9d9445f3-73fc-4b42-996d-0ef94986a351n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8kAjCHEugXX9w6Dv4uyNCUR2va938ahNaqzYtEH1cpbRA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...