Re: [MW:35031] welder qualification

6inch means 2.75inch to unlimited and thickness 2t

On Wed, 29 May 2024, 11:00 Manikandan J, <mechmani22@gmail.com> wrote:
Dear Saleem,

Please refer Table 10.9 of AWS D1.1 2020 Edition 

Regards,
Manikandan.
Abudhabi

On Wed, May 29, 2024, 8:44 AM saleem manhappulath <saleemm9526@gmail.com> wrote:
Dear All

i am going to qualifying welder on pipe as per AWS D1.1

My question is if i qualify on 6" X 10.97, electrode e 6010 root+hot & e 7018 rest . whats is the qualification range for dia and thickness 



Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3OmtsQGJggFHLALaMyUJL%3DGzX2a3_zysrqKOz4n%2BvuFRs5A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPdGVmMW4YhYk0Jx%3DSJw-3vb7q30G-CYGb7S5%2BcW9vE3un6tTg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHt4qw87B%3DJdXe-%2Br5rwgToB6dOd221UQOjptC3f2PnKygviUA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...