Re: [MW:35025] Use of Low alloy steels at high temps

475 may not happen in low alloy steel.
Sigma phase formation will happen when --if %Cr-16%C/%Ni,     Less than 1.7, No sigma phase,  if it is more than 1.7 , Sigma phase
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Mon, May 20, 2024 at 11:10 AM Talha Aamir <aamirtalha01@gmail.com> wrote:
Hi fellows,
I wanted to know why low alloys are used in high temperature service and how they resist damage mechanisms like 475C embrittlement, HTHA, Graphitization. I guidance regarding reasons behind their selection other than cost savings.

Thanks.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABXHva4qF7QEC6YkO3B7gwAEu7wekFu2uYfHW1FSHD48Zod%2BBA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNmM8yoDPoXRvqq%2BKO69AkfbS8bjMScSo8Y6QuO7j6wQg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...