Re: [MW:35008] Impact test

MDMT 

On Fri, May 17, 2024 at 9:50 AM saleem manhappulath <saleemm9526@gmail.com> wrote:
Dear team

   What is impact test? , what is the reason to do that?, how to select impact temperature for each material?, 

Non aramco and aramco 

Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

From iPhone xs

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3Omv%3DVHBp6v-XuNWuJQuq%2B9waiwKmixJbJFNCQ68%3DGLwyGw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGAT7zetip7JtPKkjmLavEgkYr8gtwvfNsqehF4q1%2BNwP%3DseyQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...