Re: [MW:35001] Cold pass

2. Normally the Root is more prone to pitting corrosion and to avoid Pitting corrosion problems and to pass the G48 corrosion test of 4g/m2, SDSS which has a higher PREN of 40 & above and higher CPT temperature is used in Root pass. Only Base material that will be in Solution annealed condition has the more stringent requirement of 1 g/m2 due to its near 50/50 Ferrite/Austenite ratio.

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



On Thursday, 16 May, 2024 at 02:23:17 pm IST, RITHVIK Suresh <rithviksuresh98@gmail.com> wrote:


Dear Experts,

1.Can anyone tell me what is meant by Cold pass in Dss/Sdss welding. Also please tell me the difference between Hotpass and Cold pass.

2.In DSS Pipeline welding Root pass is being performed with SDSS consumable and rest is performed with DSS consumable.  Can anyone explain me why it is performed like this

Thank you 
Rithvik 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f287cd81-3502-4980-892d-b924ca005c86n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...