Re: [MW:34994] Difference of 2% of Chromium Content on the Actual PMI VS Sec IIA

Kindly get client specification for the same as they have mentioned the acceptance criteria in the same.

Many clients are acceptable the tolarnce range is +- 10%.

In this case Chromium range between 19.8 to 28.6 is acceptable. 


On Thu, 16 May 2024, 11:53 am Ahmed Fouad, <dahan71@gmail.com> wrote:
You can make a weight analysis to insure the real content of Cr.
Knowing that this test is a destructive test.
thank you

‫في الخميس، 16 مايو 2024 في 9:35 ص تمت كتابة ما يلي بواسطة ‪Macario Jr. Palola‬‏ <‪macario.palola@gmec.ph‬‏>:‬
Sirs,

May I ask your valuable inputs with regards to my queries.
Base on the attached report, the actual value of %Cr is 20% as per PMI and the value of %Cr in ASME Sec IIA. Now my question, is this acceptable or not ?

Thank you in advance.

Regards,

Mac

The information contained in this email is intended for use only by the recipient to whom or which this is addressed. Such information may be privileged, confidential, and/or proprietary subject to the GMEC Email Disclaimer. Moreover, as we value your privacy, we will handle and safeguard any personal data we receive in this email in accordance with our Privacy Notice.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a98f67f1-0f70-4e02-ac62-785bd8abddf1n%40googlegroups.com.


--
Eng. Ahmed Fouad
Production Manager

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEKBjLjtxU5L%2B-%3DXMsJ3TepganXFkb4Esv%2BtNK%3DO-XE85KyyrA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGJf7So5VRhoAOWcbtdAEv-HnDVR1HqzwfYCHcYRe%2BRwUyZ%2Bdg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...