Re: [MW:34988] Use of SMAW at online leakage

1. GTAW is slow process since the travel speed is less and in positional welding  it is associated with High Heat Input.
2. Online leakage performed with Backing Plate hence SMAW is considered less cost, higher production rate with high travel speed and low heat input.

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



On Tuesday, 14 May, 2024 at 05:11:43 pm IST, Talha Aamir <aamirtalha01@gmail.com> wrote:


Hello everyone,
I wanted to ask why SMAW is used in online leakage rectification? Why isn't GTAW used in such cases? Do we always use SMAW in such cases?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABXHva7wSobT8RDfbcWSo2tcLRx1i2DZE6A522qYoOT8_7MTwQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...