Dear ,.

- for not getting troubles during welding a low heat input is required as much as you could
- ASTM A 1106 is not listed in ASME 8 or sec 9 ( unlisted material ) .. mechanical testing requirement should be by agreement with client
- u can use EFeMn-F or E   to match the base metal chemical .
- u have to consult the plate supplier regarding the best technique for welding and forming as it is easy for losing the mechanical prosperities benefits if formed or welded in non proper way    

Best Regards ,
ENG. Ahmed Osman



On Tuesday, May 7, 2024 at 05:55:40 p.m. GMT+3, PARAI Reaction Channel <saravanshyla@gmail.com> wrote:


Dear Sirs,

We are in the bidding stage for a project in Korea and I heard that the material will be High Manganese Austenitic Steel ( HMAS ) and copied the main properties for your review.

I have tried the welding datas for GTAW, SMAW, FCAW, SAW , the SFA No. and the AWS Class as per ASME Sec II C, brand names etc in the google search.  But I was not able to find it.

Is HADFIELD Manganese Austenitic Steel , the other name of HMAS ?

Please advise and share welding related info. for this material.

I need to select welding consumables and will do PQR in the near future.

image.png

Thanks and Regards,
Saravanan Sornam,
ANSAN-Si,
Korea.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALV1rk%2BzTj%2Bcf7UYs_FLJRT%2BiX2SUEYGrBmYXAS8iXfdy4BTZA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...