Dear,

The impact value of carbon steel SA 106 Gr B, often expressed as Charpy V-notch (CVN) impact test values, can vary depending on factors such as the specific heat treatment, testing temperature, and sample orientation. However, a common minimum requirement for SA 106 Gr B is an average absorbed energy value of 20 ft-lb (27 J) at room temperature.

This value indicates the amount of energy absorbed by the material during fracture in the Charpy V-notch impact test. It's an important measure of the material's toughness and its ability to withstand sudden loading or impact.

For precise impact values, it's advisable to refer to the material's specific requirements as outlined in relevant standards or specifications, as they may vary slightly depending on the source or application.

Regards,

AB


On Tue, 7 May 2024 at 17:26, Manish Kumar <mkmkr431@gmail.com> wrote:
Hi,
Please share the impact value of carbon steel SA 106 Gr B.


Regards
Manish Kumar 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHfQ4k6n2KTYcBFpAXdGOfh_4zF_a%3DggpuXXhecaP-Bmju0Tuw%40mail.gmail.com.


--
Best regards,

Amol K.B
B.E(Mech), CSWIP 3.2.2, NACE CIP 1 & ASNT LII(4M)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAADcG1py_aUpPh0FnxjO6V12uhocGAVUFHhzUohJrGYJWxUFDQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...