Dear,

Certainly, according to AWS D1.1, the qualification of Procedure Qualification Record (PQR) for pipes is indeed possible. The relevant clause in AWS D1.1 that addresses this is typically Clause 3, "Qualification." This clause outlines the requirements and procedures for qualifying welding procedures, including those for pipes.

To qualify a PQR for pipe welding under AWS D1.1, you would need to follow the guidelines outlined in Clause 3, which includes considerations for thickness, diameter, and testing requirements.

Here's a summary of what AWS D1.1 typically requires for qualifying pipe PQRs:

  1. Thickness Range: Specify the range of pipe thicknesses for which you intend to qualify the procedure. AWS D1.1 usually provides guidelines for the minimum and maximum thicknesses that can be included in the qualification.

  2. Diameter Range: Similar to thickness, specify the range of pipe diameters for which you intend to qualify the procedure. This may vary based on project requirements and industry standards.

  3. Testing Requirements: AWS D1.1 typically specifies the testing requirements for qualifying welding procedures. This may include various non-destructive testing (NDT) methods such as ultrasonic testing (UT), radiographic testing (RT), magnetic particle testing (MT), or dye penetrant testing (PT), depending on the specific welding process and material.

To provide specific qualification ranges for thickness, diameter, and testing, it's important to refer directly to the AWS D1.1 code for the most up-to-date and accurate information. Additionally, consulting with a qualified welding engineer or inspector can help ensure that the qualification process aligns with the requirements of AWS D1.1 and any other applicable codes and standards.

Regards,

AB


On Tue, 7 May 2024 at 14:14, saleem manhappulath <saleemm9526@gmail.com> wrote:
Dear All

   I have situation, kindly advise the solution 

Can we qualify PQR in pipe in AWS. D1.1. If we can please suggest qualification range . Thickness , dia and testing 

Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

From iPhone xs

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3Oms3iAKJnAg2Am7Ysx7RswowxX5zAPaiAnkrgEFZ8X7_Fw%40mail.gmail.com.


--
Best regards,

Amol K.B
B.E(Mech), CSWIP 3.2.2, NACE CIP 1 & ASNT LII(4M)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAADcG1qbc5gLqqvX4%3Do0WmXPenKSJ4y-QG92%2BFUBc-9s6vb2hQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...