Carbon steel is often used in boiler feed water lines due to its cost-effectiveness and suitability for high-pressure, high-temperature applications. However, the choice between carbon steel and stainless steel (SS) depends on several factors:

  1. Cost: Carbon steel is generally more affordable than stainless steel, making it a preferred choice for large-scale projects where cost is a significant consideration.

  2. Strength and Durability: Carbon steel is known for its strength and durability, especially in high-pressure environments. It can withstand the stresses associated with boiler feed water systems.

  3. Corrosion Resistance: While stainless steel (SS) offers superior corrosion resistance compared to carbon steel, the feed water quality and operating conditions play a crucial role. If the feed water is properly treated and maintained within acceptable parameters, carbon steel can perform adequately without significant corrosion issues.

  4. Compatibility: Depending on the specific composition of the feed water (e.g., pH levels, dissolved oxygen content), carbon steel may be sufficiently compatible. However, in cases where the feed water contains corrosive elements or impurities, stainless steel might be a better choice due to its higher corrosion resistance.

  5. Maintenance Requirements: Stainless steel generally requires less maintenance compared to carbon steel because of its superior corrosion resistance. However, carbon steel can still be effectively maintained through proper monitoring, inspection, and maintenance practices.

In summary, carbon steel is often used in boiler feed water lines due to its cost-effectiveness, strength, and suitability for high-pressure applications. However, the choice between carbon steel and stainless steel depends on various factors such as cost, corrosion resistance requirements, and operating conditions.



On Mon, 6 May 2024 at 18:45, Talha Aamir <aamirtalha01@gmail.com> wrote:
Hi,
Why we use Carbon steel in Boiler feed water lies? Why not SS?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABXHva5YnfaxAPCr3n_hw3MJ_NLdshac%2BGiu06R9G520MrzR3Q%40mail.gmail.com.


--
Best regards,

Amol K.B
B.E(Mech), CSWIP 3.2.2, NACE CIP 1 & ASNT LII(4M)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAADcG1od85NmPj3QyjXUnJ9oG8JD8qh7Mdj9dH1E66XU4uFKvA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...