this is not fully answer to your very elaborative question, but in short,

1. Low-alloy steels contain alloy element Cr, Mo, V, Ni
2. Low-alloy steels has a balanced compositions of above alloy element to resist  475C embrittlement, HTHA, Graphitization. 

On Monday, May 20, 2024 at 8:41:07 AM UTC+3 Talha Aamir wrote:
Hi fellows,
I wanted to know why low alloys are used in high temperature service and how they resist damage mechanisms like 475C embrittlement, HTHA, Graphitization. I guidance regarding reasons behind their selection other than cost savings.

Thanks.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/88e2c303-d2e4-4ba2-aae5-b725bee3bae0n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...