Tuesday, May 14, 2024

[MW:34984] Moderator's spam report for materials-welding@googlegroups.com

This message is being sent to you because you are a moderator of the group materials-welding.

The following suspicious messages were sent to your group, but are being held in your moderation queue because they are classified as likely spam messages.

If you take no action, all the messages below will be discarded automatically as spam.

However, if you see any messages that are not spam below, you may approve them individually by going to:

https://groups.google.com/group/materials-welding/pendmsg

Please do not mark this notification as spam; this is a service for group moderators. If you do not wish to receive these notifications in the future, you may change your preferences by going to:

https://groups.google.com/group/materials-welding/manage_post


------- 1 of 2 -------
Subject: Re: [MW:34982] waiting period between welding and NDT
From: Vignesh Manoharan <vkemano@gmail.com>
Date: May 13 07:04PM +0530

24hrs for GTAW and 48hrs for SMAW.



On Mon, 13 May, 2024, 6:44 pm Ali Aghajafari, <aghajafari.ins@gmail.com>
wrote:



Approve: https://groups.google.com/group/materials-welding/pendmsg?view=full&pending_id=828453974921601543

------- 2 of 2 -------
Subject: Re: [MW:34982] waiting period between welding and NDT
From: Mtho Kana <khazimlakana@gmail.com>
Date: May 13 04:54PM +0200

Recommended is anything from 12 to 24 hours.

Best Regards

On Mon, May 13, 2024 at 3:14 PM Ali Aghajafari <aghajafari.ins@gmail.com>
wrote:



Approve: https://groups.google.com/group/materials-welding/pendmsg?view=full&pending_id=5578857596811916084


For more information about this message, please visit:
https://support.google.com/groups/answer/2466386

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...