[MW:34965] Urgent request - High Manganese Austenitic Steel ( HMAS )- GTAW , SMAW datas -

Dear Sirs,

We are in the bidding stage for a project in Korea and I heard that the material will be High Manganese Austenitic Steel ( HMAS ) and copied the main properties for your review.

I have tried the welding datas for GTAW, SMAW, FCAW, SAW , the SFA No. and the AWS Class as per ASME Sec II C, brand names etc in the google search.  But I was not able to find it.

Is HADFIELD Manganese Austenitic Steel , the other name of HMAS ?

Please advise and share welding related info. for this material.

I need to select welding consumables and will do PQR in the near future.



Thanks and Regards,
Saravanan Sornam,
ANSAN-Si,
Korea.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALV1rk%2BzTj%2Bcf7UYs_FLJRT%2BiX2SUEYGrBmYXAS8iXfdy4BTZA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...