316 - C:0.08max UTS : min 75ksi
316L - C:0.03 max UTS : min 70ksi
For dual certified both the conditions to be satisfied.
Dual certified 316/316L - C: 0.03 max UTS : min 75ksi
Thanks & Regards
J.Gerald Jayakumar
0091-8838619635
On Monday, 29 April, 2024 at 08:05:51 pm IST, duybien.com <bck055@gmail.com> wrote:
Dual grade complied type 316 and 316L.
- Chemical composing of %C: < 0.03%, and
- Min. YS: 205 MPa.
Regards
On Thursday, April 25, 2024 at 4:35:46 PM UTC+7 kumar sumit wrote:
Dear expert,What is the meaning of dual grade lile 316/316L. Van anyone explain.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/9a3429f5-740c-4d61-8d6e-cb63f4782390n%40googlegroups.comhttps://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
.
Comments