310 is fully Austenitic structure,  u may land into fissuring.  u may go with 316l or 309MoL

On Wed, Apr 17, 2024, 7:35 PM PARAI Reaction Channel <saravanshyla@gmail.com> wrote:
Dear Welding Experts,

To weld SS 310 to SS 316L material, can I use GTAW SFA 5.9, AWS Class ER310 ?

Or which AWS class will be suitable to weld this dissimilar materials ?

Please advise with valuable reasons as per metallurgy.

Thanks and Regards,
Saravanan Sornam,
ANSAN-Si,
S.Korea.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALV1rkJr5HQjGy3waKzgUajF4y6BPosROzpxawfUWzi%3D6_zgRA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNfGkP0y_dPi%3Dvp1-XE4xoHnXxHdT-bpRHjsFNYMNjcGQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...