[MW:34899] Vessel Leg & Base Plate Impact Test

Dear All,

When constructing a vessel where Impact Testing is applicable, should Impact Tests also be conducted on the welds of the Leg and Base Plate (non-pressure parts)?

The Project specification only outlines requirements applicable to the vessel, such as temperature or pressure. 


If Impact Testing needs to be applied to Leg & Base Plate, which paragraph of the code should be referenced?

If it is not required to apply Impact Testing, which paragraph of the Code should be referenced?  


Thank you
Regards,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8f1ed1c9-1cf2-48eb-b2e7-8fdcd9043684n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...