Re: [MW:34880] PWHT of Normalized head

Hi, 
If you heat treated 900°C , then no need to do 610°C. 

On Mon, 15 Apr 2024, 4:05 pm anthony chundal, <anthony.chundal@gmail.com> wrote:
Hi

PWHT is required for 45 thk, normalizing is separate heat treatment and cant be combined with stress relieving,

Regards,



On Sun, Apr 14, 2024 at 4:56 PM Muhammed Ibrahim PK <ibratech@gmail.com> wrote:
Gentlemen,

Is PWHT can be avoided if the welded head (2 piece construction) performs normalizing after forming ?

Head MOC : SA516 Gr 70, 45 mm thk, fabricated by welding the blank in two pieces. 

Complete vessel not required PWHT.

Thanks & Regards
Muhammed Ibrahim PK

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALOPgmMorLP3zvhePLHgVGFbcpx-t-%2BSd3M6EQpsfpHrAs38Ow%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOi%3DZp_yfMnLqJsy9WdQhYq%2B24k2an4dznaaYgJH-GHGRbWcDw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEabyKk7%2BZva7ZY1EZmHWHXELJ04%2BDprqb_tkQ%2BKmQ9YG-Kb1Q%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...