For fillet,  I don't think 38 mm pqr is needed for asme ix compliance


This 38 mm requirement comes from qw-202.3 which is more for weld repair and build up and qualifying unlimited parent material thickness. Also , please see qw-202.4

On Wed, 17 Apr 2024, 11:14 Shivasankar A, <shivasankar2593@gmail.com> wrote:
Dear team,

can anyone clarify my issue.

During the preparation of WPS & PQR of SA 516 GR 70 to SA 516 GR 70 - 10mm Plate Groove weld, my AI (Authorised Inspector) was insisted me to put the Thickness range for fillet weld as 38mm maximum in both WPS & PQR. 

I am unable to understand this. Because as per ASME Section IX Table QW451.4 - All groove weld tests can qualify "All fillet sizes on all base metal thicknesses and all diameters" So according to my understanding it should be unlimited but why my AI insisting me to put as 38 mm max..

Pls Clarify.

Regards,
Shivasankar A

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b568812e-6355-43a5-8574-0fc6a039a5acn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACpSjO%3DKgWEUeR17w0H2z8Ns83VPi0qqT-KputCmEaJR0tHm4g%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...