Sunday, April 21, 2024

[MW:34870] ASME IX, groove weld during WQT limits for Fillet Weld production

For ASME IX, in general, I am aware that a groove weld during WQT will qualify for all thicknesses for actual production's fillet weld.
However, is there a minimum required thickness for this groove weld during WQT?

We used a 5 mm plate for WQT groove weld, Single-V, GTAW + SMAW. GTAW by other welder/before WQT; The GTAW pass was about 4mm and the SMAW (excluding capping/reinforcement) was just 1 mm. Does this 1 mm pass qualify us to weld ALL thicknesses for fillet weld during production for the SMAW process?

During production, the joints are all T-Joint fillet weld using SMAW process.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c839e465-a50d-4032-ae64-eea5cab790can%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...