Saturday, April 20, 2024

Re: [MW:34874] PWHT of Normalized head

If dish normalised no need to do PWHT.

On Mon, 15 Apr 2024, 1:34 pm atul jha, <atulkrjha21@gmail.com> wrote:
Kindly get a data from design team for fiber elongation if code of construction is divViii and if it is grater then 10 percent PWHT is mandatory.
Regards 
Atul

On Sun, Apr 14, 2024, 15:56 Muhammed Ibrahim PK <ibratech@gmail.com> wrote:
Gentlemen,

Is PWHT can be avoided if the welded head (2 piece construction) performs normalizing after forming ?

Head MOC : SA516 Gr 70, 45 mm thk, fabricated by welding the blank in two pieces. 

Complete vessel not required PWHT.

Thanks & Regards
Muhammed Ibrahim PK

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALOPgmMorLP3zvhePLHgVGFbcpx-t-%2BSd3M6EQpsfpHrAs38Ow%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC1tTULwuM3xTxWod9V%3Df8o%2BXGUom8Td7odGa04mCwo8YKiMzg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEabyK%3DFzV0XXXETE6STwTxjDKf6FNZi5PBsrV%2BQ0iAddpandA%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...