Re: [MW:34847] Submerged Arc Welding Process Wire/Flux Classification

Dear prashant

That is corect

When you will prepare PQR with impact test and SAW process for carbon steel, you should be check temperature and compare with table 7 of ASME sect. IIC part SFA A5.17

Hope this can answer your question

Salam
Kurniatullah,IWE


Pada Kam, 4 Apr 2024, 16.51, Prashant <pprane.rane1@gmail.com> menulis:
For SAW welding wire/flux classification as an sample for discussion

As per A 5.17 it is represented as F7P8-EH12K, this classification is given by the product manufacturer on the flux bag and is inline with the ASME Sec II Part C SFA 5.17
Where P is pwht and 8 is Minus 80 Deg F Impact test

I have a Procedure qualification which is Impact tested at Minus 50 Deg F, Qualified as per ASME Sec IX
as per QW 404.9
is it correct I write on my Procedure qualification record
F7P5-EH12K

Please advise above is correct,  if not I would like to understand more on this what should be written and clarification to increase knowledge

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f81d62f2-1e20-456f-baee-0159e2ef3222n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFo4ueoxqHBdngQrG2Gjm6Jb7SKxGdif%2BeRZhjFv-YRdj4s5Kg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...