[MW:34930] Re:

Dual grade complied type 316 and 316L.
- Chemical composing of %C: < 0.03%, and
- Min. YS: 205 MPa.

Regards


On Thursday, April 25, 2024 at 4:35:46 PM UTC+7 kumar sumit wrote:
Dear expert, 
                      What is the meaning of dual grade lile 316/316L. Van anyone explain. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---