Skip to main content

[MW:34743] HP Drum Internal Parts Inspection & Repair

Dear Exports,

We have spotted a cracks on the shell to dished head joints, CS1 & CS2.

We plan to cut out the CS1 & CS2 joints completely since the cracks are all over the joint. Then, remove all cracks and perform NDT and re-welding of the joints.

Our concern is the difficulty in performing hydrostatic tests. Please let us know if the hydrostatic test is mandatory after repair. The drum has Several nozzles connected to different parts of the HRSG and main steam headers. Hence, blinding of the nozzles would be challenging. Please let us know if we can use any alternative method instead of the Hydrostatic test.

BR,
MIDHUN

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6460a54b-3add-4c85-bd71-47769b965f42n%40googlegroups.com.

Comments

Firoze said…
Dear Midhun,

In My Opinion,

It's Better to do Hydro Test after Major Repair (In High Pressure Drum)

If Client Not Required Hydro Test & If Client Accept With NDT - You can waive off

Client Confirmation is Main

Thanks

Best Regards
Firoze
BV-ADH





Thanks
Best Regards
Firoze

Firoze said…
Dear Midhun,

In My Opinion

If Any Repair Carried out after Hydro Test

Hydro Re-Test To Be Carried out along with Repair Joint NDT Reports.


Getting Client Approval Prior to these is Good Practice.
(client acknowledgement is Important)


Thanks

Best Regards
Firoze
BV-AUH

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...