Re: [MW:34600] Plug Welding

Groove weld WPS cannot be used in tube to tube sheet welding in heat exchanger Tube replacement . Separate WPS need to be prepared as per ASME SEC 9 and also the welder need to be qualified using that WPS 

On Tue, 24 Oct 2023 at 4:12 PM Ashish Chacko <iamashleo007@gmail.com> wrote:
I have a question regarding the use of a groove weld WPS for plugging a tube in an exchanger and whether it is necessary to qualify a Tube-to-Tubesheet (TTS) WPS instead. I would greatly appreciate your insights on this matter.

As per my understanding since it is a fillet weld we can do. If not please provide me reference.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0554da58-cb54-469e-b60d-1210621da32en%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB9mKLQof4DJ6%3DLiyXQnVS76ge8R66LF9UaGhS6KAr75fvR44w%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...