Tuesday, October 24, 2023

Re: [MW:34600] Plug Welding

Ashish 
You can use the groove qualified WPS 
Enure ASME sec IX requirements are met 
Essential ,Non essential ,Supplentary  variables 
Thanks 
Vishwas IWE 
Sent from my iPhone

On 24-Oct-2023, at 6:42 PM, Ashish Chacko <iamashleo007@gmail.com> wrote:

 I have a question regarding the use of a groove weld WPS for plugging a tube in an exchanger and whether it is necessary to qualify a Tube-to-Tubesheet (TTS) WPS instead. I would greatly appreciate your insights on this matter.

As per my understanding since it is a fillet weld we can do. If not please provide me reference.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0554da58-cb54-469e-b60d-1210621da32en%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...