Re: [MW:34590] Welder Qualification

Mean he is qualified for CS & SS Both. 

On Mon, 16 Oct, 2023, 12:52 pm John, <johnmounir20002000@gmail.com> wrote:
Can a welder use SS electrode on CS material ? for qualification and what is the range?
thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/96f58af9-2886-4359-99c7-b6ff1faddbc6n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC6cZ-jafAFXzgpmm6WtcNSiHTGyv5MspsXxJDPJcJDn8C3hKg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...