Re: [MW:34582] QW 406 , preheat maintenance

Preheat maintenance, Maintain the Preheat temp till completion of welding, due to short term power cut etc.  Post heating/ Hydrogen Bake out, is after completion  of welding,  The weldment shall be held at temperature above the preheat temperature  for some time to release the hydrojen
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Mon, Oct 9, 2023 at 12:24 PM mithlesh kumar <mithleshmech47@gmail.com> wrote:
Then what is the difference between post heating and pre heat maintenance.

On Friday, June 27, 2014 at 12:02:24 PM UTC+5:30 george....@gr.bureauveritas.com wrote:

Preheat maintenance, according to ASME IX,  is not post heating
Preheat maintenance means that you do not cool down before perform PWHT
B31.1 requires preheat maintenance for Pno15E unless engineering provides differently

    best regards

    Dr. Georgios Dilintas

    Authorized Nuclear Inspector
    Authorized Inspector Supervisor


    I&F REGIONAL TECHNICAL MANAGER
    BUREAU VERITAS HELLAS

    Tel: +30 210 40 63 113/4
    Fax: +30 210 40 63 118
    Cell: +30 69 44 64 62 04
    (See attached file: Dilintas_George.vcf)

Inactive hide details for Kannayeram Gnanapandithan ---27/06/2014 08:01:37---since max welding is taken place SMAW, it is betteKannayeram Gnanapandithan ---27/06/2014 08:01:37---since max welding is taken place SMAW, it is better to go for POST Heat . temp 50degree above ur pre



From: Kannayeram Gnanapandithan <kgpan...@gmail.com>
To: materials-welding <material...@googlegroups.com>
Date: 27/06/2014 08:01
Subject: Re: [MW:21275] QW 406 , preheat maintenance
Sent by: material...@googlegroups.com





since max welding is taken place SMAW, it is better to go for POST Heat . temp 50degree above ur preheat temp and time for minimum 30minutes

THANKS & BEST REGARDS
KG.PANDITHAN, AWS-CWI, CSWIP 3.1
CONSULTANT-WELDING & QUALITY


On Thu, Jun 26, 2014 at 11:09 PM, Mahantesh Loni <mahan...@gmail.com> wrote:

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/78049824-566b-4208-9a8b-b59e0c428479n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNDVRiCnJJbpzs819W%2BtewgffXd_XxUp1J3jotyk_COFw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...