Re: [MW:34562] MOC-316L ,P-8 ,FILLET WELD PROCEDURE QUALIFICATION

Dear all,

According to ASME Section IX, macro testing is typically not required for fillet weld qualification, regardless of the material specification, including stainless steel like SS 316L. Paragraph QW-202.2(c) of ASME Section IX states: 

"For fillet weld qualification in accordance with QW-202.3, macroscopic examination is not required." This means that macro testing, which involves the preparation and examination of cross-sectional samples of the weld's internal 

structure, is not necessary for the qualification of fillet welds, even when dealing with materials like SS 316L. 


Best regards,


Le lun. 2 oct. 2023 à 13:59, SIDDIQUE IMAM <sddqimam@gmail.com> a écrit :
Dear expert,

As per ASME sec-9 , QW-202.2 para C ,
We can proceed SS-316L Material GTAW, FILLET WELD PROCEDURE QUALIFICATION, please suggest me if macro test is applicable for this requirement.
Because my job is only fillet weld small bore socket type welding required for my scope of work.

Fillet‐weld
procedures so qualified may be used for welding all thick-
nesses of base metal for all sizes of fillet welds, and all dia-
meters of pipe or tube in accordance with Table
QW-451.4. Nonpressure‐retaining fillet welds, as defined
in other Sections of the Code, may as an alternate be qual-
ified with fillet welds only. Tests shall be made in accor-
dance with QW-180. Limits of qualification shall be in
accordance with Table QW-451.3.

Kindly update ASAP.


With warm Regards,

SIDDIQUE IMAM
QA/QC ENGINEER
MOB: +91-7600972964 
EMAIL- sddqimam@gmail.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHNDPiM_SGL31%3DNuc-uNW2d5ydXiUhUkKk92Sbqs5AhaoWj18w%40mail.gmail.com.


--

Mostafa DAIF
Chef preparateur

T : 05 23 38 90 72
M : 06 61 54 12 95
TAQA MOROCCO PB 99 Sidi Bouzid - El Jadida 24 000 - Maroc
taqamorocco.ma

TAQA MOROCCO is a member of the Abu Dhabi National Energy Company Group of companies.
  

The information contained in this communication is confidential, may be attorney-client privileged, and is intended only for the use of the addressee. It is the property of Abu Dhabi National Energy Company PJSC (TAQA) or one of its affiliates. Unauthorized use, disclosure or copying of this communication or any part thereof is strictly prohibited and may be unlawful. If you have received this communication in error, please notify me immediately by return email and destroy this communication and all copies thereof, including attachments.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANRRH0LZQCOyrNKf-8J-k8E37qOEJ0Pmft_DiLGtkeoCS1%2Bxfg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...