[MW:34584] Required chemical composition for carbon & low-allot steel and stainless steel per NACE MR0175/2021

Hi experts,

 

This is related to chemical composition of carbon and low alloy steel per NACE MR0175-2021

Chemical composition for carbon and low alloy steel

Per Clause A.2.1.2 - Carbon & low-alloy steel are acceptable at 22 HRC max. hardness provided they contain less than 1% mass fraction Nickel.

Per Clause 8 -    Max. acceptable level for flat-rolled produce is 0.003% mass fraction of sulfur

Max. acceptable level for seamless product is 0.01% mass fraction of sulfur

Conventional forgings with sulfur levels less than 0.025% mass fraction and castings are not considered sensitive to HIC and SOHIC

 

Is this the only minimum required chemical composition for carbon & low-alloy steel?

Can you please suggest the clause for chemical composition for stainless steels as well?


Regards,

Akash Wagh.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKx5G%3DbFbjopChQ%3D6xOC7FKgyC%3DtQXwyVK3kDMK5pCapxPHofw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...