Hi

If WPS Qualified for Groove welds also qualified for fillet weld only want to check for thickness rank for approved WPS.

Regards
Ramamoorthi Thangarasu

On Tue, Oct 24, 2023 at 6:42 PM Ashish Chacko <iamashleo007@gmail.com> wrote:
I have a question regarding the use of a groove weld WPS for plugging a tube in an exchanger and whether it is necessary to qualify a Tube-to-Tubesheet (TTS) WPS instead. I would greatly appreciate your insights on this matter.

As per my understanding since it is a fillet weld we can do. If not please provide me reference.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0554da58-cb54-469e-b60d-1210621da32en%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEE6Dzdu6b9pvt4_tHpSdaGaFnH%3DbWbejK%3DmzeJuQYCgNSs0Lw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...