Monday, October 9, 2023

Re: [MW:34577] Excess weaving in FCAW welding process

Yes, as per drawing design temperature is 0 degree celsius.  

Best Regards,
Rajesh

On Fri, Oct 6, 2023 at 12:52 PM Vishwas Keskar <vvkeskar123@gmail.com> wrote:
Is impact testing is required as per drawing ??

Sent from my iPhone

On 05-Oct-2023, at 7:30 PM, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:


welder became in fatigue stress in handling the torch. 18mm is the dia of nozzle approximately 

On Mon, Oct 2, 2023, 6:29 PM RAJESH KUMAR <rajeshkumarbhaskara@gmail.com> wrote:
Dear Experts,

Code:BSEN 15614-1:2017 ,BSEN 15609:2019 and DNV-OS-C401

I have noticed that WPS says the weaving is allowed/permitted 18 mm maximum for FCAW welding process.Please tell me whether we can allow if the weaving is more than the allowable limit.If it can be allowed.What is the reasons and on what basis it is allowed?If it can not/should not be allowed.Why and what is the reasons?


Thanks & Regards

Rajesh kumar
Dubai.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMtcSfPVaUrZpa-zbt1cQ0%3DcLD5g6OuEVPkDv36KTkbeZUsghg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOQ_of%2B70TZqnZoZzfEZQznihOzPKeYLjfEH3RcjrDkCg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/07038A05-0267-4420-ABD5-1F7D826BCD02%40gmail.com.


--




Best Regards,
Rajesh Kumar
Dubai.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMtcSfM1Xbo%3D2xPVvv-kEhaz-aWB-egmrwWCWm9c0m2M%2B%3Df9ZA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...