Saturday, October 14, 2023

[MW:34586] Thicker Plate 4mm SS304L bevel preparation

Dear Expert,

Please advise bevel preparation for 4mm plate to plate weld, to avoid distortion.Please advise if any procedure can i refer.


Thank you, Regards
Helmi,

  

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHjDVH8%2BdkF7EGk3UfbGEcvhNxVw5e70twB7edKo7i1ThxVHDg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...