Re: [MW:34577] How to calculate Repair percentage

Greetings
Below here is repair rate farmula 

% RR = (Lr/ Lw) X 100
where:
% RR = percent repair rate.
Lr = welder's total length of repairs in one week, mm
Lw = welder's total length of weld radiographed in one week, mm

Muhammad Babur Khan

Sent from my iPhone

On 9 Oct 2023, at 9:54 AM, Karuppa Samy <samyqc08@gmail.com> wrote:

Dear experts,

how to calculate radiography repair percentage for 100% RT joints and random RT joints. please explain with applicable reference standard

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/855522fb-714e-4f59-916f-da475471e4b2n%40googlegroups.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...