42CrMo4 material is equivalent to ASTM 4140. 


On Mon, Oct 16, 2023 at 1:15 PM Ritesh Kumar Singh <riteshsiwan770@gmail.com> wrote:
Dear Sir,
I thought Er90S-B3  is used for low alloy 

On Mon, 16 Oct, 2023, 12:52 pm Parminder Singh, <parmsin2021@gmail.com> wrote:
GTAW ER 90S-B3 
SMAW E 11070 

On Fri, Oct 13, 2023, 22:30 SANJAY SINGH <sanjay.kharwar349@gmail.com> wrote:
Can any one tell me about selection fo welding consumables for 42CrMo4 material with E250 BR 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4205fd8d-e84f-4655-a2f2-1a8eb59dee97n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGAT7zcZ-w%2Bng3G%3Dram7MDwwL3%2ByTk4zTNmix2DHiba8HqBCsg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC6cZ-iKm5ryDp8HARKwaDdgbbMtUS3URMNSMPZNFWYXpbXPGQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGAT7zfzm2xDv5Bx-Yb3K4FAze0yfcxzRot%2Bazw_ZrW2VZ-%2BLQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...