Re: [MW:34577] How to calculate Repair percentage

The repair percentage for 100% RT Joints may be calculated by the below 3 methods as recommended in the Client Specification.

1. Joint Wise - Number of Joints Defective / Total Number of Joints Radiographed x 100
2. RT Film Wise - Number of Repair Films / Total Number of Films Radiographed x 100
3. Length Wise  - Length of Repair / Total Length Radiographed x 100

Acceptance Limits as per Client Specification.

Random RT depends on Applicable Code + Client specification.

Example of ASME B31.3 as below.

Inline image

Penalty for defective Joints as per Applicable Client Specification.

Thanks & Regards

J.Gerald Jayakumar



On Monday, 9 October, 2023 at 12:24:52 pm IST, Karuppa Samy <samyqc08@gmail.com> wrote:


Dear experts,

how to calculate radiography repair percentage for 100% RT joints and random RT joints. please explain with applicable reference standard

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/855522fb-714e-4f59-916f-da475471e4b2n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...