Re: [MW:34096] Forming marks on Dish End of pressure vessel

I think 3rd Party Who released this Vessel must be contacted to confirmed their out put. It end surface area shall be smooth. 



On Thu, 23 Mar 2023, 08:25 Vasagan Balaji, <7vasagan@gmail.com> wrote:
In 22 years of experience, Myself alone inspected more than 1k U stamped pressure vessels but never encountered as such enclosed. Strange ! Better to consult some reputed third party agencies.

On Thu, 23 Mar, 2023, 9:26 am , <ameerbashasheikh@gmail.com> wrote:
Hi, 

One of our pressure vessel manufacturer recently supplied Oil and Gas separator having distinct forming marks on dish ends. Supplier claims that those marks are aesthetic and do not hamper vessel performance. Photo is attached herewith. 

Being the end user we are not in position to make final decision whether to accept the pressure vessel with distinct marks on dish ends and put under operation or not. The pressure vessel is designed as per ASME sec VIII Div I and vessel is U Stamped. The vessel is hydro tested and holds good. ASME inspector has not commented anything on forming marks or pressing marks in their release note. 

Please guide should we accept it or to ask supplier to rectify the same or any section of ASME code confirms non acceptance of same in pressure vessel. 

Regards, 
Ameer Basha 

image0.jpeg

image1.jpeg

Sent from my iPhone

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/12B831C2-EDD1-42CB-B64F-B9BAE4EAFC60%40gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKV0Q%2BjRu0czN353Dv%2Btpnq62BDVZUBKhfLStLk1A6y41FzdrQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHqH7yDx2WnKQcwNZ49thgj6itzxnDZ6FHpj7SLTbk_eyEb3FA%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...