Wednesday, March 15, 2023

[MW:34066] Causes of patterning after machining (A182 F316 Forging material)

Dear Expert,

As you can see in the photo below, after finishing machining (roughness - Max. 63 AARH), a grain-like pattern occurs on the surface.

IMG_3459.jpg

What could be the cause of this phenomenon?

I would appreciate your expert advice.

--
https://materials-welding.blogspot.com/