Dear Experts 
Good afternoon ,
Background - 
SS 304L -18 mm  plate is cladded with MONEL 400  by explosion bonding.(6mm)
Ellipsoidal dished end is to be  formed (570mm ID).

PFHT  by virtue of operating conditions is not envisaged .

Seeking guidance for :
Pl. Suggest  
1)Cold forming or 
2) Hot forming 

Pl. suggest suitable process/any heat treatment  with supporting Code/Book reference
Appreciate if somebody Shares any experience  with similar combinations

Thanks 
Vishwas - IWE 



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ad7d9227-2082-42c7-ab52-6f7b756edf60n%40googlegroups.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...