[MW:34033] Re: Regarding weld overlay with ECuNi 90/10 with the WPS ECuNi (70/30)

This non ferrous weld metal.
What is the F number of PQR  filler metal?
If PQR filler metal's F number and Production joint filler metal's F number  is same ,then new PQR is not required 
Thanks
Vishwas -IWE 
On Friday, February 24, 2023 at 3:23:47 PM UTC+5:30 mohit aggarwal wrote:
Dear Experts,

We have equipment of weld overlay with 90/10 CuNi composition, but we have Procedure is only with 70/30 CuNi consumable.

As per QW-404.37 clause our AI asked to requalify the procedure due to change of consumable.

I have query can we do weld overlay of 90/10 with 70/30 consumable or we will have qualify new procedure for the same.


Regards,
Mohit Aggarwal
Welding Engineer

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/111d0d70-5570-42f9-8bfe-b914bf7c01b8n%40googlegroups.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...