[MW:34063] SA 765 Grade II ( Normalize + Temper)

Dear Expert,

Kindly advice 
for subjected material I want to qualify PQR P1G2 ( normalize) to P1G2 ( normalize + temper) for impact application.

As lead time for forging SA 765 gr 2 is quite high I want to perform tempering on plate SA516 gr 70 (Normalize) to simulate actual condition of N+ T before welding.

Kindly  advice soaking time calculation for tempring cycle  @ 670 deg cel.
Plate thick 50 mm

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOdsS43OxMNM6jxErQzfzfAx2vgxSXyz1YuC_avrsoR69XZ%2B-Q%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...