Re: [MW:34080] E 7018 and E 8010-B2 IN SAME BAKING OVEN

Electrode type indicates whether low H2 Basic / Cellulosic / Rutile and also includes as material type such as carbon steel / SS.

In your case, you can use the same oven.

Thanks & Regards

J.Gerald Jayakumar



On Monday, 20 March, 2023 at 04:23:26 pm IST, Aneesh K <aneeshknair87@gmail.com> wrote:


Hi Folks,

Could any experts clarify regarding the subject matter, if it is allowed to keep both E7018 and E 8018-B2 electrodes in the same Baking/ Holding oven for conditioning purposes.
As required by Saudi Aramco Standard SAES-A-206. section 7.7.1, """"Electrodes shall be properly stored and segregated in the store, shop, or ovens to avoid mix-up. Separate ovens are required for different welding consumable types.""""

Please clarify if E7018 and E8018-B2 are to be considered as different type of electrodes from 
Baking point of view 



Thanks and Regards

Aneesh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFWZHfnzJU4K%3DoHLBotqv4QVrGfKzKPakyiMvAAi2xGxMjp%3DQA%40mail.gmail.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...