On Thu, Mar 2, 2023 at 5:11 AM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Use 316Ti, for 6CrNiMoTi 17122. and for 13CrMo 4-5 either NiCr3 or 309 ( based on service Temp)
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Wed, Feb 22, 2023 at 9:12 AM Anand Elankumaran <email2uranand@gmail.com> wrote:
Dear Experts,

Could you Please advise if the below consumable selection is correct or not.

WPS Requirements as per BS EN 15609 & 15614

Material

Size

Process(Est. Weld thk)

Material Grouping  as per PD CR ISO 15608

Suitable Consumable

Remarks

GTAW

SMAW

1.4571EN  X 6 CrNiMoTi 17 122 to
1.4571EN  X 6 CrNiMoTi 17 122

22.3 X 2.77

GTAW (2.77)

8.1

ER 316L-17

--

(Exaton 316/316L-17)

1.4571EN  X 6 CrNiMoTi 17 122 to
1.4571EN  X 6 CrNiMoTi 17 122

168.3 X 10.97

GTAW + SMAW (4 + 6.97)

8.1

ER 316L-17

E 316L-17

(Exaton 316/316L-17)

1.7335EN, 13CrMo4-5 to
1.4571EN X 6 CrNiMoTi 17 122

33.4 X 3.38

GTAW (3.38)

8.1 - 5.1

ER NiCrMo-3

--

 

 


--
Thanks and Regards,
E. Anand,
Lead QA-QC,
Sohar,
Oman.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANOYChwvFgCTrAHGN4Jp62zbaUGPfo%3D2YjVi7Vn8y44q9eufcQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNFMDnEksFYoUNmh%2BM%2Ba4LkFJpkWjhxWELKMX3WZ5%2B0WQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVihNFadeA%2BFLxx5PphQuQMAFfv5rPUYrRN%3Dt%3DUNWbDv%2Bj3w%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...