Friday, March 3, 2023

Re: [MW:34050] FILLER WIRE FOR SA516 GR.70 TO SB409UNSNO8810

u can use ERNiCrMo3
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Mar 2, 2023 at 4:25 PM sujit kumar <sujitkumar19942@gmail.com> wrote:
Dear sir 
thank you for your reply....But  ENiCrFe-3  is the electrode but i want to know fiiler metal....Please reply.



Best Regards
S.k

On Thu, 2 Mar 2023 at 13:05, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
pls use ENiCrFe-3 and it also depends on the Design Temperature



On Thursday, 2 March, 2023 at 11:06:55 am IST, sujit kumar <sujitkumar19942@gmail.com> wrote:


Dear all,

What filler wire we have to use to welding of SA516 GR.70 TO SB409UNSNO8810




Best Regards.
S.K

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFonYWMxEnVrD2tCb4CXihObGTnhBLX02cFe8L0KQNePCCezMA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1208277335.1767262.1677739622866%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFonYWNkNO-nmq_KJ8dOMOmsKyN-R5PY5BT8YcS1BATt8th63A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNZ0bpWeLkU9Vo2hJW8wmJuTsm4s8_XbkDttLSFVA6SgA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...