Re: [MW:34071] Clarification Required

Not posible to correspond P number to material not included in Section IX.
Only will be qualified for the specific material.

Regards 

El vie, 17 mar 2023, 13:25, Madhava Ram <madhav.ram56@gmail.com> escribió:
Dear Team,
As per ASME Sec IX 2021
IS 2062 E350 is an unassigned grade whish is not listed in the QW/QB_422 but our client is insisting us to add the material in P1 and G2 to perform the PQR and WPS qualification.
Kindly share your option on this

Thanks in Advance
--
With Regards,


Madhavaram E
(+91) 9486940897

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPtDbpq5A5%3Dw3hANsL33zZ0gX3_1jWF1JxBiJ1eQGcb4phXPQA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKxkP8fLc%2B995ysZ972cXkVSQ17k6azSXwcP0KhJMM1pkkiL-Q%40mail.gmail.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...