Re: [MW:33999] PWHT time

The rate of Heating / Cooling to be considered.
Approximately  250 Deg Celsius per hour for Carbon steel. 


Regards
V.Kingsly Geo

On Mon, 10 Oct 2022 at 10:26, Muhammed Aaftab Khan Pathan <aaftab.khan2222@gmail.com> wrote:
Soaking time 6 hours + 1 hr heating time + 1 hr cooling time = 8 hours total PWHT Cycle time.

On Sat, 8 Oct 2022, 14:15 Student, <nabeel233@gmail.com> wrote:
The following is an exam question. Please guide how to do it

A  one and Half inch of material has to be PWHTed from 600 F to 1350  and shall be kept at 1350 F for 6 hours. It has to be cooled down back to 600 F. If the rate of heating and cooling is 500F per hour per inch  , what is the total time for PWHT.  Do not consider heating the material up to 600F in the calculation

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/472dc2c2-2914-4cb4-abf5-a400e882886fn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEjHOtDs2uyAH3fRV7AjEWxUG4kCzpfEEGTFYJi%3Dry%3Dz4i7ihg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAR7VZ8A%2B5uaMXWNMfd3vYSVYQTJ7Q_m3FZJVmfRAZYNA5rOkw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...