Re: [MW:33993] Prequalification of WPS as per AWS D1.1 - PIPE TO PIPE BUTT JOINT(PJP)

Pre Qualifed WPS is available.  Check the joint types 

On Friday, December 16, 2022 at 9:02:01 AM UTC+3 Sandeep wrote:
Dear Sham,


Please refer Fig 5.2 (Page#113 in AWS D1.1:2020 Edition) for the Joint details. Prequalified WPS can be prepared for this joint configuration.

With Regards,

SANDEEP RAGHAVAN

INSPECTION ENGINEER

linkedin icon



On Thu, Dec 15, 2022 at 8:06 AM Sham Shahabuddin -Welding Inspector, HANBO <shamshahab...@gmail.com> wrote:
Dear Experts

Please input your suggestions and comments for my condition below

Joint: Pipe to Pipe corner 45 degrees - Butt 
Size: 4" sch 40 astm A53
Standard: AWS D1.1
Application: Guard Rail
Welding Process: SMAW.

My question is whether prequalified WPS is available for this condition in AWS D1.1 if PJP is used. If available, please let me know with the reference. When I search I'm unable to find any reference with regards to diameter ranges for the prequalified WPS.

image.png
Thanks and Regards
SHAM SHAHABUDDIN
QC INSPECTOR - WELDING

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAyAb6Niu%2B%2BS%3Dq%2BNY-8Tw19WsE6mE7eMTzezyNK-omwwrHCDqg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/00d4d29d-d78f-4a47-ba03-7f35f1287fabn%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...