Thursday, February 2, 2023

Re: [MW:33982] Pressure guage range

Inline image


Thanks & Regards

J.Gerald Jayakumar



On Thursday, 2 February, 2023 at 09:08:43 am GMT+3, binit kumar <ishwarbinit@gmail.com> wrote:


Dear Mr. Sourav,
Greetings of the Day.

Kindly check ASME BPVC VIII, UG-102 for pressure  gauge reference.

Regards,
Binit Kumar
CSWIP-3.1 Qualified

On Thu, Feb 2, 2023 at 8:42 AM Sourav Bohrays <souravbohrays@gmail.com> wrote:
Dear experts
Kindly provide clause for pressure guage range for hydro test as per asme b31.3.


Regards
Sourav

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOWr6k-8CBmAAYdUhGaxz0Fcb1nP431c%2BKyTOhRbqrJ4vHaG2Q%40mail.gmail.com.


--
BINIT KUMAR
+918717929495

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJ0ob9Aejmq-_Jm7fkoRaW%3Dq%2BpHQ5SuqQ3feteeOQhWQcHLwpg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...