Could you Please advise if the below consumable selection is correct or not.

WPS Requirements as per BS EN 15609 & 15614

Material

Size

Process(Est. Weld thk)

Material Grouping  as per PD CR ISO 15608

Suitable Consumable

Remarks

GTAW

SMAW

1.4571EN  X 6 CrNiMoTi 17 122 to
1.4571EN  X 6 CrNiMoTi 17 122

22.3 X 2.77

GTAW (2.77)

8.1

ER 316L-17

--

(Exaton 316/316L-17)

1.4571EN  X 6 CrNiMoTi 17 122 to
1.4571EN  X 6 CrNiMoTi 17 122

168.3 X 10.97

GTAW + SMAW (4 + 6.97)

8.1

ER 316L-17

E 316L-17

(Exaton 316/316L-17)

1.7335EN, 13CrMo4-5 to
1.4571EN X 6 CrNiMoTi 17 122

33.4 X 3.38

GTAW (3.38)

8.1 - 5.1

ER NiCrMo-3

--

 

 


--
Thanks and Regards,
E. Anand,
Lead QA-QC,
Sohar,
Oman.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANOYChwvFgCTrAHGN4Jp62zbaUGPfo%3D2YjVi7Vn8y44q9eufcQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...